Oxidation behavior of Nb-24Ti-18Si-2Al-2Hf-4Cr and Nb-24Ti-18Si-2Al-2Hf-8Cr hypereutectic alloys at 1250℃

    在线阅读 下载PDF 导出详情
    摘要 Nb-24Ti-18Si-2Al-2Hf-4CrandNb-24Ti-18Si-2Al-2Hf-8Cralloyswerepreparedbyarcmeltinginawater-cooledcrucibleunderargonatmosphere.Microstructuralcharacteristicsandoxidationresistanceofthealloysat1250℃wereinvestigated.Theresultsshowthat,whentheCrcontentis4at%,themicrostructuresconsistof(Nb,Ti)_(ss)andNb_5Si_3;asCrcontentincreasesto8at%,C14LavesphaseCr_2Nbisformed.Theisothermaloxidationtestsshowthattheoxidationkineticsofthetwoalloysfollowsimilarfeatures.Theweightgainsofthetwoalloysafteroxidationat1250℃for100hare235.61and198.50mg·cm~(-2),respectively.Duringoxidation,SiO_2,TiO_2,Nb_2O_5andCrNbO_4areformedatfirst.Then,Ti_2Nb_(10)O_(29)isformedafteroxidationfor20minandbeginstochangeintoTiNb_2O_7astheoxidationproceeds.SiO_2isformedassolidstateatfirstbutlaterevolvesintoglassystatetoimprovethecohesionofthescale.Afteroxidationfor100h,oxidationproductsconsistofSiO_2,TiNb_2O_7,Nb_2O_5andCrNbO_4.
    机构地区 不详
    出处 《稀有金属:英文版》 2017年3期
    出版日期 2017年03月13日(中国Betway体育网页登陆平台首次上网日期,不代表论文的发表时间)
    • 相关文献
    Baidu
    map