Toeffectivelysolvetheagglomerationproblemsinthesolidstatereactionprocess,pre-addingglucoseisadoptedtothesynthesisofLiFePO4/CenergymaterialsusingFe–Pwasteslag.Theaverageparticle&grainsizeofLiFePO4/Cdecreases,andtheimpuritiesinLiFePO4/Ccompositesreducetoagreatextent.Itmakesgreatsensetothemassindustrialproduction.Theoptimumsynthesisconditionsdeterminedinthisworkarebasedontheorthogonalexperiments.Thesamplessynthesizedinascaleof500gexhibithighpurity,excellentelectrochemicalperformance,highreactionactivity,goodreversibility,andlowpolarizationlevel.Thedischargecapacitiesare145,134,117,and102mAh/gatthecurrentdensitiesof0.1C,0.2C,0.5Cand1C,respectively.ThisworkputsforwardapracticalsuggestionformassproducingenvironmentalbenignandlowcostLiFePO4/Cascathodematerialsoflithiumionbatteries.